SCC crack initiation of alloy 82 in hydrogenated steam at 400 degrees c - Centre de mathématiques appliquées (CMAP) Accéder directement au contenu
Communication Dans Un Congrès Année : 2015

Dates et versions

cea-02500826 , version 1 (06-03-2020)

Identifiants

  • HAL Id : cea-02500826 , version 1

Citer

C. Guerre, J. Crepin, M. Sennour, C. Duhamel, E. Heripre, et al.. SCC crack initiation of alloy 82 in hydrogenated steam at 400 degrees c. Réunion annuelle de l'ICG EAC, May 2015, Ann Harbor, United States. ⟨cea-02500826⟩